Amorphous and crystalline phases in superdispersed diamond have been determined by thermogravimetric analysis at a heating rate 1.25 K min−1 or lower, and the kinetic parameters of oxidation of different carbon species have been calculated.
References
1.
10.1070/MC1999v009n05ABEH001123_bib1
Lyamkin
Dokl. Akad. Nauk SSSR,
1988
2.
10.1070/MC1999v009n05ABEH001123_bib2
Vereshchagin
Sbornik dokladov V Vsesoyuznogo soveshchaniya po detonatsii (Proceedings of the Fifth All-Union Conference on Detonation),
1991
3.
10.1070/MC1999v009n05ABEH001123_bib3
Tatsii
Sbornik dokladov V Vsesoyuznogo soveshchaniya po detonatsii (Proceedings of the Fifth All-Union Conference on Detonation),
1991
4.
10.1070/MC1999v009n05ABEH001123_bib4
Mal’kov
Proceedings of the American Physical Society Conference ‘Shock Compression of Condensed Matter’ Seattle,
1995
5.
A. L. Vereshchagin, E. A. Petrov, G. V. Sakovich, V. F. Komarov, A. V. Klimov and N. V. Kozyrev, US Patent 5861349, 1999.
6.
10.1070/MC1999v009n05ABEH001123_bib6
Vereshchagin
Sverkhtverdye Materialy,
1990
7.
T. M. Gubarevich, I. S. Larionova, R. R. Sataev, V. Yu. Dolmatov and V. F. Pyaterikov. USSR Inventor's Certificate 1819851, 1992.
8.
Freeman E.S., Carroll B.
The Journal of Physical Chemistry,
1958
9.
10.1070/MC1999v009n05ABEH001123_bib9
Gubarevich
Zh. Prikl. Khim.,
1991
10.
10.1070/MC1999v009n05ABEH001123_bib10
Vereshchagin
Sverkhtverdye Materialy,
1992